<rt id="kmlev"></rt><rt id="kmlev"></rt><bdo id="kmlev"><delect id="kmlev"><rt id="kmlev"></rt></delect></bdo><rt id="kmlev"></rt><noframes id="kmlev"><rt id="kmlev"></rt><noframes id="kmlev"><delect id="kmlev"></delect><noframes id="kmlev"><rt id="kmlev"><delect id="kmlev"></delect></rt><noframes id="kmlev"><delect id="kmlev"></delect><noframes id="kmlev"><delect id="kmlev"></delect> <noframes id="kmlev"><rt id="kmlev"></rt><noframes id="kmlev"><rt id="kmlev"></rt><rt id="kmlev"><rt id="kmlev"></rt></rt><noframes id="kmlev"><rt id="kmlev"></rt><rt id="kmlev"><delect id="kmlev"></delect></rt><noframes id="kmlev"><rt id="kmlev"></rt><rt id="kmlev"></rt><rt id="kmlev"></rt><rt id="kmlev"></rt> <rt id="kmlev"><rt id="kmlev"></rt></rt><rt id="kmlev"></rt><bdo id="kmlev"><delect id="kmlev"><noframes id="kmlev"><noframes id="kmlev"><rt id="kmlev"><delect id="kmlev"></delect></rt><rt id="kmlev"></rt><rt id="kmlev"></rt><rt id="kmlev"><delect id="kmlev"><delect id="kmlev"></delect></delect></rt>
封邊機

PUR全自動封邊機

  由于板材封邊工藝受到很多的外界以及機器因素的影響,導致封邊質量差,一直是各工廠比較頭疼的問題。
  
  1、選用厚的封邊帶封邊時,封邊機壓料輪位置應根據邊條厚度調整至最佳。由于封邊帶比工件稍長,當壓料輪壓住封邊帶長出部分時,給封邊帶一個垂直于進給方向的力,此時由于膠還未完全固化,膠合強度不高,尾部易松開而粘貼不牢固。
  
  2、封邊機工作室內溫度不能過低,一般應在12℃以上。封邊帶越厚,柔韌性越差,要保證預熱裝置的正常工作,若無預熱裝置時也可采用電吹風加熱等方法使封邊帶軟化。加工車間內不得有過堂風。
  
  同時封邊帶的自身質量也會影響封邊效果,質量好的封邊帶封出的效果接縫嚴密,質量差的封邊帶封出的產品封邊處縫隙較大,有明顯的黑線。較厚的封邊帶從斷面看,邊帶中部應稍微比兩邊凹一些,經過壓帶輪擠壓過后,與板材結合更緊密,無縫隙。
  
  3、實木類的含水率不要過高,板材應儲存在陰涼和干燥的室內,含水率在8-10%為最佳。保持基材表面無灰塵,干凈。
  
  4、機器封邊時輸送速度很快,熱熔膠在低壓力下要具有很好的彌散性和對基材的滲透性,良好的初粘性,在短時間壓力作用下瞬間膠合,粘貼牢固。使用時要注意保證熱熔膠的溫度在正常溫度范圍內,長時間過高的溫度會使膠快速氧化發硬;而過低的溫度下熱熔膠又會流動性不好,出現斷膠現象。
  
  5、涂膠量大小控制,應該以板材、邊帶結合處外邊略擠出膠為準。如果膠量過大,封邊處余膠嚴重,影響美觀;過小,粘合強度不夠。檢驗涂膠是否連續均勻,可用普通封邊帶封邊,趁膠未冷卻時將封邊帶迅速撕掉,看板材表面,及邊帶表面存膠情況。
  
  6、封邊機沒有安裝預銑裝置的,板材的切割質量,是非常影響封邊效果的。一般廠家使用推臺鋸下料,切割板材時都會使用刻痕鋸,成品切割完,最佳效果是切割面處能看到小鋸片痕跡,但摸起來卻感覺不到。也就是說,小鋸片的切割寬度應該比主鋸片寬0.1毫米(兩側各0.05毫米),并且主副鋸片在同一水平線上。小鋸片開槽太寬導致板材下方粘貼不牢固,封邊處產生黑線或者有明顯縫隙。小鋸片開槽過小,又會導致板材爆邊,影響封邊效果。

標簽: 全自動封邊機 板材 PUR